1.1 This test method is used to measure the thermal-protective properties of materials that provide thermal insulation when contact is made with hot surfaces during a limited exposure up to 1 min.
1.1.1 During this limited time exposure, the temperature can reach a threshold approaching 600 °F (316 °C).
Author | ASTM |
---|---|
Editor | ASTM |
Document type | Standard |
Format | File |
ICS | 13.340.10 : Protective clothing
|
Number of pages | 7 |
Replace | ASTM F1060-16 + Redline |
Set | ASTMVOL1103 |
Year | 2018 |
Document history | ASTM F1060-16 + Redline |
Country | USA |
Keyword | ASTM 1060;ASTM F1060;ASTM F1060;10.1520/F1060-18 |